← Fiberglass course syllabus

Assessment and preparation · Lesson 5 of 22

Map gelcoat cracks and impact damage

Start wide enough to show the fitting, molding or hull feature around the mark. Then take a close view with a scale and oblique light. Draw the direction of each crack and note any impact history. A star pattern is evidence of geometry; it does not establish the depth of damage.

Impact center · Radiating cracks (schematic)

Workshop exercise

Make a damage map with the boat side, a fixed reference and the date. Compare a later image from the same angle. If fibers are exposed, the panel moves, or the damage is near a loaded attachment, bring the record to a qualified repairer.

Hull inspection
Hull inspection · Boatyard context

Check your understanding

Why photograph before grinding or filling?

Show the reasoning

Preparation can erase the original pattern and the clues needed to understand the cause.

Further reading · WEST SYSTEM Fiberglass Boat Repair & Maintenance manual